Fig. 5From: Tribological properties of nanolamellar tungsten disulfide doped with zinc oxide nanoparticlesFriction coefficient versus time for undoped nanolamellar WS2 at 25 and 400 °C, nanolamellar WS2 doped with n-ZnO at 25 and 400 °CBack to article page