Table 6 Experimental conditions and results

From: Optimization of wear loss in silicon nitride (Si3N4)–hexagonal boron nitride (hBN) composite using DoE–Taguchi method

Expt. no.

Load (N)

% hBN

Expt. result-WVL (mm3/m)

1

50

8

4.01204

2

100

8

5.0456

3

150

8

5.0498