Table 3 Average values analysis of liquid iron and molten steel

From: Effect of shrouding CH4 flow rate on flow field and stirring ability of coherent jet in steelmaking process

Label

Liquid iron

Molten steel

Steelmaking time (min)

C (%)

P (%)

Temperature (°C)

C (%)

P (%)

[C]·[O] (10−4)

Temperature (°C)

10 %-CH4

3.6

0.129

1280

0.078

0.007

0.0053

1605

50.3

8 %-CH4

3.6

0.130

1279

0.079

0.007

0.0052

1606

50.4

6 %-CH4

3.6

0.129

1280

0.081

0.010

0.0061

1605

54.1