Fig. 8From: The electrospinning of the copolymer of styrene and butyl acrylate for its application as oil absorbentThe morphology of the fibrous membrane electrospun from the spinning solution of the synthesized polymer 1# at an extrusion rate of 0.8 ml/h; V1# prepared at an applied voltage of 12 kV; V2# prepared at an applied voltage of 15 kV; V3# prepared at an applied voltage of 18 kVBack to article page