From: Effect of vertically aligned carbon nanotube density on the water flux and salt rejection in desalination membranes

Fig. 2

VACNT membrane fabrication process. a VACNT on silicon substrate glued to glass. b PDMS is added. c PDMS is cured through heating in a vacuum oven, and the volatile part of the PDMS is evaporated. d Silicon and glass substrates are removed using mechanical peeling. e VACNT–PDMS composite is sliced using a microtome machine. f Photograph of one of the developed VACNT membranes