Fig. 8From: Dynamic recrystallization behavior and processing map of the Cu–Cr–Zr–Nd alloyProcessing maps for the Cu–Cr–Zr–Nd alloy at a true strain of: a 0.3; b 0.4; c 0.5 and d 0.6Back to article page