Table 1 Detailed POSS-PANI composite samples

From: Porous POSS-PANI nanofibre from interfacial polymerization and hydrothermal approach

Sample ID

OAPS concentration (mol %)

Details

POPA-1

0.5

Interfacial polymerization, 25 °C, pH = 3.0

POPA-2

1.0

POPA-3

1.5 

POPA-4

2.0 

POPA-5

2.0 

24-h hydrothermal treatment

POPA-6

2.0 

48-h hydrothermal treatment

POPA-7

2.0

96-h hydrothermal treatment