Fig. 7From: The electrospinning of the copolymer of styrene and butyl acrylate for its application as oil absorbentThe morphology of the fibrous membrane electrospun from the spinning solution of the synthesized polymer 1# at an applied voltage of 15 kV; R1# prepared at an extrusion rate of 0.4 ml/h; R2# prepared at an extrusion rate of 0.8 ml/h; R3# prepared at an extrusion rate of 1.2 ml/hBack to article page